Effect of Cement Replacement by Bauxite Residue on Mechanical Properties of Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Cement Replacement by Bauxite Residue on Mechanical Properties of Concrete

Author(s): Yassine Brahami, Mathieu Fiset, Ali Saeidi, Kadiata Ba, and Rama Vara Prasad Chavali

Publication: Materials Journal

Volume: 122

Issue: 1

Appears on pages(s): 19-30

Keywords: bauxite residue; cement; mechanical properties

DOI: 10.14359/51744374

Date: 1/1/2025

Abstract:
Concrete, a highly energy-intensive material, contributes approximately 10% of global carbion dioxide (CO2) emissions. To address this issue, incorporating industrial residues in concrete production has emerged as a viable solution, reducing natural resource consumption and lowering the CO2 footprint. Using bauxite residues in concrete has proven to be an environmentally friendly and sustainable approach. In this study, cement mass was partially replaced with bauxite residues (at 5%, 10%, 15%, and 20%), with variations in residue diameter (300 μm, 600 μm, and 2 mm) and in liquid form. The concrete’s workability, air content, density, mechanical strength, elasticity, Poisson’s ratio, and porosity were assessed with each replacement percentage. The study revealed that bauxite residues can effectively replace up to 20% of cement in a concrete mixture. Although their use slightly affects the fresh properties of concrete, it significantly enhances its mechanical properties. With this approach, a sustainable and eco-friendly concrete without compromising its performance can be created.

Related References:

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 624 pp.

Anagnostopoulos, A.; Navarro, M. E.; Stefanidou, M.; Ding, Y.; and Gaidajis, G., 2021, “Red Mud-Molten Salt Composites for Medium-High Temperature Thermal Energy Storage and Waste Heat Recovery Applications,” Journal of Hazardous Materials, V. 413, p. 125407. doi: 10.1016/j.jhazmat.2021.125407

Atan, E.; Sutcu, M.; and Cam, A. S., 2021, “Combined Effects of Bayer Process Bauxite Waste (Red Mud) and Agricultural Waste on Technological Properties of Fired Clay Bricks,” Journal of Building Engineering, V. 43, p. 103194. doi: 10.1016/j.jobe.2021.103194

Bayat, A.; Hassani, A.; and Azami, O., 2018, “Thermo-Mechanical Properties of Alkali-Activated Slag–Red Mud Concrete,” Road Materials and Pavement Design, V. 21, No. 2, pp. 411-433. doi: 10.1080/14680629.2018.1500299

CSA A23.1-19, 2019, “Concrete Materials and Methods of Concrete Construction,” CSA Group, Toronto, ON, Canada.

CSA A23.2-19, 2019, “Test Methods and Standard Practices for Concrete,” CSA Group, Toronto, ON, Canada.

CSA A23.3-19, 2019, “Design of Concrete Structures,” CSA Group, Toronto, ON, Canada.

Di Mare, M.; Monteiro, V. N.; Brial, V.; Ouellet-Plamondon, C. M.; Fortin, S.; Tsesmelis, K.; Montini, M.; and Rosani, D., 2021, “A Calculator for Valorizing Bauxite Residue in the Cement Industry,” Journal of Cleaner Materials, V. 1, p. 100009. doi: 10.1016/j.clema.2021.100009

fib, 2010, fib Model Code for Concrete Structures 2010, Ernst and Sohn, Lausanne, Switzerland.

Hong, Q.; Wang, P.; Chen, Z.; Huang, Z.; Shen, L.; and Song, T., 2021, “Evaluation of Red Mud as Oxygen Carrier for Chemical Looping Combustion of Methane and Biomass in Fluidized Bed,” Fuel Processing Technology, V. 222, p. 106964. doi: 10.1016/j.fuproc.2021.106964

Hossain, M. U.; Cai, R.; Ng, S. T.; Xuan, D.; and Ye, H., 2021, “Sustainable Natural Pozzolana Concrete–A Comparative Study on its Environmental Performance against Concretes with Other Industrial By-Products,” Construction and Building Materials, V. 270, p. 121429. doi: 10.1016/j.conbuildmat.2020.121429

Illavarason, P.; Renjit, A.; and Mohan Kumar, P., 2018, “Clinical Evaluation of Functional Vision Assessment by Utilizing the Visual Evoked Potential Device for Cerebral Palsy Rehabilitation,” Procedia Computer Science, V. 132, pp. 128-140. doi: 10.1016/j.procs.2018.05.174

Kumar, A., and Kumar, S., 2013, “Development of Paving Blocks from Synergistic Use of Red Mud and Fly Ash Using Geopolymerization,” Construction and Building Materials, V. 38, pp. 865-871. doi: 10.1016/j.conbuildmat.2012.09.013

Liu, C.-J.; Li, Y.-Z.; Luan, Z.-K.; Chen, Z.-Y.; Zhang, Z.-G.; and Jia, Z.-P., 2007, “Adsorption Removal of Phosphate from Aqueous Solution by Active Red Mud,” Journal of Environmental Sciences, V. 19, No. 10, pp. 1166-1170. doi: 10.1016/S1001-0742(07)60190-9

Liu, R.-X., and Poon, C.-S., 2016, “Utilization of Red Mud Derived from Bauxite in Self-Compacting Concrete,” Journal of Cleaner Production, V. 112, pp. 384-391. doi: 10.1016/j.jclepro.2015.09.049

Liu, X.; Han, Y.; He, F.; Gao, P.; and Yuan, S., 2021, “Characteristic, Hazard and Iron Recovery Technology of Red Mud - A Critical Review,” Journal of Hazardous Materials, V. 420, p. 126542. doi: 10.1016/j.jhazmat.2021.126542

Milačič, R.; Zuliani, T.; and Scancar, J., 2012, “Environmental Impact of Toxic Elements in Red Mud Studied by Fractionation and Speciation Procedures,” The Science of the Total Environment, V. 426, pp. 359-365. doi: 10.1016/j.scitotenv.2012.03.080

Panda, I.; Jain, S.; Das, S. K.; and Jayabalan, R., 2017, “Characterization of Red Mud as a Structural Fill and Embankment Material Using Bioremediation,” International Biodeterioration & Biodegradation, V. 119, pp. 368-376. doi: 10.1016/j.ibiod.2016.11.026

Paramguru, R. K.; Rath, P. C.; and Misra, V. N., 2004, “Trends in Red Mud Utilization – A Review,” Mineral Processing and Extractive Metallurgy Review, V. 26, No. 1, pp. 1-29. doi: 10.1080/08827500490477603

Paultre, P., 2017, Structures en Béton Armé: Analyse et Dimensionnement, V. 2, Presses Internationales Polytechnique, Montreal, QC, Canada.

Raj, R. K., and Rajab, P. M., 2018, “Effect of Red Mud and Iron Ore Tailings on the Strength of Self Compacting Concrete with Polypropylene Fibre,” International Journal of Civil Engineering and Technology, V. 9, No. 13, pp. 456-471.

Rio Tinto, 2016, “PUBLIC CONSULTATION REPORT on the Vaudreuil Project beyond 2022,” https://transfertconsult.ca/wp-content/uploads/2017/02/Rapport_consultation_Vaudreuil_au-dela_2022_VF4.pdf. (in French) (last accessed Dec. 18, 2024)

Shetty, K. K.; Nayak, G.; and Vijayan, V., 2014, “Effect of Red Mud and Iron Ore Tailings on the Strength of Selfcompacting Concrete,” European Scientific Journal, V. 10, No. 21.

Song, Y.; Dong, M.; Wang, Z.; Qian, X.; Yan, D.; Shen, S.; Zhang, L.; Sun, G.; Lai, J.; and Ruan, S., 2022, “Effects of Red Mud on Workability and Mechanical Properties of Autoclaved Aerated Concrete (AAC),” Journal of Building Engineering, V. 61, p. 105238. doi: 10.1016/j.jobe.2022.105238

Sun, Y.; Li, J.-S.; Chen, Z.; Xue, Q.; Sun, Q.; Zhou, Y.; Chen, X.; Liu, L.; and Poon, C. S., 2021, “Production of Lightweight Aggregate Ceramsite from Red Mud and Municipal Solid Waste Incineration Bottom Ash: Mechanism and Optimization,” Construction and Building Materials, V. 287, p. 122993. doi: 10.1016/j.conbuildmat.2021.122993

Sunitha, M. P., and Prakash, K. B., 2014, “Effect of Replacement of Cement by Red Mud on the Properties of Concrete,” International Journal of Scientific and Engineering Research, V. 5, No. 9, pp. 805-814.

Tang, W. C.; Wang, Z.; Donne, S. W.; Forghani, M.; and Liu, Y., 2019, “Influence of Red Mud on Mechanical and Durability Performance of Self-Compacting Concrete,” Journal of Hazardous Materials, V. 379, p. 120802. doi: 10.1016/j.jhazmat.2019.120802

Tang, W. C.; Wang, Z.; Liu, Y.; and Cui, H. Z., 2018, “Influence of Red Mud on Fresh and Hardened Properties of Self-Compacting Concrete,” Construction and Building Materials, V. 178, pp. 288-300. doi: 10.1016/j.conbuildmat.2018.05.171

Wang, S.; Jin, H.; Deng, Y.; and Xiao, Y., 2021, “Comprehensive Utilization Status of Red Mud in China: A Critical Review,” Journal of Cleaner Production, V. 289, p. 125136. doi: 10.1016/j.jclepro.2020.125136

Ye, J.; Hu, A.; Ren, G.; Chen, M.; Tang, J.; Zhang, P.; Zhou, S.; and He, Z., 2018, “Enhancing Sludge Methanogenesis with Improved Redox Activity of Extracellular Polymeric Substances by Hematite in Red Mud,” Water Research, V. 134, pp. 54-62. doi: 10.1016/j.watres.2018.01.062


ALSO AVAILABLE IN:

Electronic Materials Journal