High-Strength Headed Bars in Joints of Special Moment Frames under Cyclic Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: High-Strength Headed Bars in Joints of Special Moment Frames under Cyclic Loading

Author(s): H.-J. Lee, F.-C. Yu, K.-C. Lin, J.-C. Wang, B. L. Worsfold, and J. F. Silva

Publication: Structural Journal

Volume: 121

Issue: 6

Appears on pages(s): 105-120

Keywords: anchorage; beam-column joint; development length; headed bars; high-strength reinforcement; joint shear; reversed cyclic loading

DOI: 10.14359/51740866

Date: 11/1/2024

Abstract:
This paper presents cyclic test results of nine beam-column joints, fabricated with Grades 60, 80, and 100 (Grades 420, 550, and 690) No. 11 (D36) headed bars in joints with matching concrete strengths. With the exception of the joint shear determination, each specimen was designed in accordance with ACI 318-14 provisions for special moment frame joints. The headed bar embedment length was determined using 1.0fy in accordance with ACI 318-14, rather than the ACI 318-19 requirement to use 1.25fy to calculate the development length. Test results demonstrate that the ACI 318-14 development length can be used for closely spaced high-strength No. 11 (D36) headed bars in joints with Code-conforming transverse reinforcement. This paper also aggregates the test data with prior research and compares the data with descriptive equations and breakout methodology for assessing the development length and anchorage strength of headed bars. The results support several design recommendations for the ACI 318 provisions.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

2. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

3. Joint ACI-ASCE Committee 352, “Recommendations for Design of Beam-Column Connections in Monolithic Reinforced Concrete Structures (ACI 352R-02) (Reapproved 2010),” American Concrete Institute, Farmington Hills, MI, 2010, 40 pp.

4. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-05) and Commentary (ACI 318R-05),” American Concrete Institute, Farmington Hills, MI, 2005, 430 pp.

5. Thompson, M. K., “The Anchorage Behavior of Headed Reinforcement in CCT Nodes and Lap Splices,” PhD dissertation, The University of Texas at Austin, Austin, TX, 2002, 502 pp.

6. Thompson, M. K.; Ziehl, M. J.; Jirsa, J. O.; and Breen, J. E., “CCT Nodes Anchored by Headed Bars - Part 1: Behavior of Nodes,” ACI Structural Journal, V. 102, No. 6, Nov.-Dec. 2005, pp. 808-815.

7. Thompson, M. K.; Jirsa, J. O.; and Breen, J. E., “Behavior and Capacity of Headed Reinforcement,” ACI Structural Journal, V. 103, No. 4, July-Aug. 2006, pp. 522-530.

8. Thompson, M. K.; Jirsa, J. O.; and Breen, J. E., “CCT Nodes Anchored by Headed Bars - Part 2: Capacity of Nodes,” ACI Structural Journal, V. 103, No. 1, Jan.-Feb. 2006, pp. 65-73.

9. Thompson, M. K.; Ledesma, A.; Jirsa, J. O.; and Breen, J. E., “Lap Splices Anchored by Headed bars,” ACI Structural Journal, V. 103, No. 2, Mar.-Apr. 2006, pp. 271-279.

10. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-08) and Commentary (ACI 318R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 465 pp.

11. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-11) and Commentary (ACI 318R-11),” American Concrete Institute, Farmington Hills, MI, 2011, 503 pp.

12. Kang, T. H.-K.; Shin, M.; Mitra, N.; and Bonacci, J. F., “Seismic Design of Reinforced Concrete Beam-Column Joints with Headed Bars,” ACI Structural Journal, V. 106, No. 6, Nov.-Dec. 2009, pp. 868-877.

13. Lee, H.-J., and Yu, S.-Y., “Cyclic Response of Exterior Beam-Column Joints with Different Anchorage Methods,” ACI Structural Journal, V. 106, No. 3, May-June 2009, pp. 329-339.

14. Kang, T. H.-K.; Kim, W.; and Shin, M., “Cyclic Testing for Seismic Design Guide of Beam-Column Joints with Closely Spaced Headed Bars,” Journal of Earthquake Engineering, V. 16, No. 2, 2012, pp. 211-230. doi: 10.1080/13632469.2011.610497

15. Chiu, C.-K.; Chi, K.-N.; and Lin, K.-C., “Experimental Investigation on the Seismic Anchorage Behavior of Headed Bars Based on Full-Size Specimens of Exterior and Interior Beam-Column Joints,” Advances in Structural Engineering, V. 19, No. 5, 2016, pp. 777-794. doi: 10.1177/1369433216630346

16. Ou, Y.-C.; Canseco, H. A.; and Kurniawan, D. P., “Anchorage Performance of Headed Deformed Bars in Exterior Beam-Column Joints under Cyclic Loading,” KSCE Journal of Civil Engineering, V. 21, No. 7, 2017, pp. 2837-2849. doi: 10.1007/s12205-017-1868-z

17. Lee, H.-J., and Chang, C.-J., “High-Strength Reinforcement in Exterior Beam-Column Joints under Cyclic Loading,” ACI Structural Journal, V. 114, No. 5, Sept. 2017, pp. 1325-1338. doi: 10.14359/51700788

18. Shao, Y.; Darwin, D.; O’Reilly, M.; Lequesne, R. D.; Ghimire, K. P.; and Hano, M., “Anchorage of Conventional and High-Strength Headed Reinforcing Bars,” SM Report No. 117, The University of Kansas Center for Research, Lawrence, KS, 2016, 334 pp.

19. Ghimire, K. P.; Darwin, D.; and O’Reilly, M., “Anchorage of Headed Reinforcing Bars in Concrete,” SM Report No. 127, The University of Kansas Center for Research, Lawrence, KS, 2018, 278 pp.

20. Ghimire, K. P.; Shao, Y.; Darwin, D.; and O’Reilly, M., “Conventional and High-Strength Headed Bars—Part 1: Anchorage Tests,” ACI Structural Journal, V. 116, No. 3, May 2019, pp. 255-264. doi: 10.14359/51714479

21. Ghimire, K. P.; Shao, Y.; Darwin, D.; and O’Reilly, M., “Conventional and High-Strength Headed Bars—Part 2: Data Analysis,” ACI Structural Journal, V. 116, No. 3, May 2019, pp. 265-272. doi: 10.14359/51714480

22. CNS 560:18, “Steel Bars for Concrete Reinforcement,” Bureau of Standards, Metrology & Inspection, Taipei, Taiwan, 2018, 12 pp.

23. ASTM A706/A706M-22, “Standard Specification for Low-Alloy Steel Deformed and Plain Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2022, 9 pp.

24. ASTM A970/A970M-16, “Standard Specification for Headed Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2016, 9 pp.

25. Kim, J., and LaFave, J. M., “Key Influence Parameters for the Joint Shear Behaviour of Reinforced Concrete (RC) Beam-Column Connections,” Engineering Structures, V. 29, No. 10, 2007, pp. 2523-2539. doi: 10.1016/j.engstruct.2006.12.012

26. Wibowo, L. S. B.; Cheng, M.-Y.; Huang, F.-C.; and Tai, T.-Y., “Effectiveness of High-Strength Hoops in High-Strength Flexural Members,” ACI Structural Journal, V. 114, No. 4, July 2017, pp. 887-897. doi: 10.14359/51689620

27. Lin, T.-H.; Chen, P.-C.; and Lin, K.-C., “The Multi-Axial Testing System for Earthquake Engineering Researches,” Earthquakes and Structures, V. 13, No. 2, 2017, pp. 165-176.

28. ACI Committee 374, “Acceptance Criteria for Moment Frames Based on Structural Testing and Commentary (ACI 374.1-05) (Reapproved 2019),” American Concrete Institute, Farmington Hills, MI, 2005, 9 pp.

29. ACI Committee 374, “Guide for Testing Reinforced Concrete Structural Elements under Slowly Applied Simulated Seismic Loads (ACI 374.2R-13),” American Concrete Institute, Farmington Hills, MI, 2013, 18 pp.

30. Ghimire, K. P.; Darwin, D.; and Lepage, A., “Headed Bars in Beam-Column Joints Subjected to Reversed Cyclic Loading,” ACI Structural Journal, V. 118, No. 3, May 2021, pp. 27-33.

31. Bashandy, T. R., “Application of Headed Bars in Concrete Members,” PhD dissertation, The University of Texas at Austin, Austin, TX, 1996, 303 pp.

32. Murakami, M.; Fuji, T.; and Kubota, T., “Failure Behavior of External Beam-column Joints with Mechanical Anchorage in Subassemblage Frames,” Concrete Research and Technology, V. 9, No. 1, 1998, pp. 1-9. doi:10.3151/crt1990.9.1_1 (in Japanese)

33. Wallace, J. W.; McConnell, S. W.; Gupta, P.; and Cote, P. A., “Use of Headed Reinforcement in Beam-Column Joints Subjected to Earthquake Loads,” ACI Structural Journal, V. 95, No. 5, Sept.-Oct. 1998, pp. 590-606.

34. Matsushima, M.; Kuramoto, H.; Maeda, M.; Shido, K.; and Ozone, S., “Test on Corner Beam-column Joint under Tri-Axial Loadings: Outline of Test: Study on Structural Performance of Mechanical Anchorage (No. 10),” Proceedings of Annual Meeting Architectural Institute of Japan, 2000, pp. 861-862. (in Japanese)

35. Nakazawa, H.; Kumagai, H.; Saito, H.; Kurose, Y.; and Yabe, Y., “Developmnet on the Ultra-High-Strength Reinforced Concrete Structure: Part 3. Loading Tests on Exterior Beam-Column Joints,” Proceedings of Annual Meeting Architectural Institute of Japan, 2000, pp. 611-612. (in Japanese)

36. Tasai, A.; Kawakatsu, K.; Kiyohara, T.; and Kubota, T., “Shear Performance of Exterior Beam Column Joint with Beam Main Bars Anchored Mechanically (Part 1): Study on Structural Performance of Mechanical Anchorage (No. 8),” Proceedings of Annual Meeting Architectural Institute of Japan, 2000, pp. 857-858. (in Japanese)

37. Yoshida, J.; Ishibashi, K.; and Nakamura, K., “Experimental Study on Mechanical Anchorage Using Bolt and Nut in Exterior Beam-Column Joint: Part 1. Specimens and Outline of Experiment,” Proceedings of Annual Meeting Architectural Institute of Japan, 2000, pp. 635-636. (in Japanese)

38. Takeuchi, H.; Nakamura, K.; Hayakawa, K.; and Ichikawa, M., “Experiments of Exterior Beam-Column Joints with Mechanical Anchorage of Circular Anchor Plate,” Proceedings of the Japan Concrete Institute, V. 25, No. 2, 2003, pp. 913-918. (in Japanese)

39. Ishibashi, K., “Experimental Study on T-shaped Beam-Column Joints Anchored by Attachments of Screw Nuts to Column Reinforcements,” Proceedings of the 13th World Conference on Earthquake Engineering,Vancouver, BC, Canada, 2004, Paper No. 1737.

40. Ishibashi, K., and Inokuchi, R., “Experimental Study on T-Shaped Joints with Anchor-Heads on Column’s Rebars,” Proceedings of the Japan Concrete Institute, V. 26, No. 2, 2004, pp. 421-426. (in Japanese)

41. Kiyohara, T.; Tasai, A.; Watanabe, K.; Hasegawa, Y.; and Fujimoto, T., “Seismic Capacity of High Strength RC Exterior Beam Column Joint with Beam Main Bars Anchored Mechanically: Part 1-4,” Proceedings of Annual Meeting Architectural Institute of Japan, 2004, pp. 27-34. (in Japanese)

42. Kiyohara, T.; Hasegawa, Y.; Fujimoto, T.; Akane, J.; Amemiya, M.; Tasai, A.; and Adachi, T., “Seismic Performance of High Strength RC Exterior Beam Column Joint with Beam Main Bars Anchored Mechanically: Part 5-9,” Proceedings of Annual Meeting Architectural Institute of Japan, 2005, pp. 33-42. (in Japanese)

43. Kato, T., “Study on Mechanical Anchorage Method Using Anchor Plate for Beam-to-Column Joints of R/C Buildings: Mechanical Anchorage Method Using Frictional Welding,” Journal of Structural and Construction Engineering (Transactions of AIJ), V. 71, No. 604, 2006, pp. 151-158. doi: 10.3130/aijs.71.151_2 (in Japanese)

44. Masuo, K.; Adachi, M.; and Imanishi, T., “Ultimate Strength of R/C Exterior Beam-column Joint using Mechanical Anchorage for Beam Reinforcement USD590—Part 1: Experiment on Anchorage Strength of Beam Reinforcement and Part 2: Experiment on Shear Strength of Beam-Column Joint,” Proceedings of Annual Meeting Architectural Institute of Japan, 2006, pp. 25-28. (in Japanese)

45. Adachi, M., and Masuo, K., “The Effect of Orthogonal Beams on Ultimate Strength of R/C Exterior Beam-Column Joint Using Mechanical Anchorages,” Proceedings of Annual Meeting Architectural Institute of Japan, 2007, pp. 633-634. (in Japanese)

46. Chun, S. C.; Lee, S. H.; Kang, T. H. K.; Oh, B.; and Wallace, J. W., “Mechanical Anchorage in Exterior Beam-Column Joints Subjected to Cyclic Loading,” ACI Structural Journal, V. 104, No. 1, Jan.-Feb. 2007, pp. 102-112.

47. Tazaki, W.; Kusuhara, F.; and Shiohara, H., “Tests of R/C Beam-Column Joints with Irregular Details on Anchorage of Beam Longitudinal Bars: Part 1: Outline of Tests; Part 2: Test Results and Discussions,” Proceedings of Annual Meeting Architectural Institute of Japan, 2007, pp. 653-656. (in Japanese)

48. Chun, S. C., and Shin, Y. S., “Cyclic Testing of Exterior Beam-Column Joints with Varying Joint Aspect Ratio,” ACI Structural Journal, V. 111, No. 3, May-June 2014, pp. 693-704. doi: 10.14359/51686730

49. Dhake, P. D.; Patil, H. S.; and Patil, Y. D., “Anchorage Behaviour and Development Length of Headed Bars in Exterior Beam-Column Joints,” Magazine of Concrete Research, V. 67, No. 2, 2015, pp. 53-62. doi: 10.1680/macr.14.00144

50. Chicchi, R.; Varma, A. H.; Seo, J.; Bradt, T.; and McCarty, E., “Experimental Testing of Tension-Loaded Deformed Anchors in Concrete,” ACI Structural Journal, V. 117, No. 5, Sept. 2020, pp. 133-146.

51. Worsfold, B. L.; Moehle, J. P.; and Silva, J. F., “Moment Transfer at Column-Foundation Connections: Physical Tests,” ACI Structural Journal, V. 119, No. 5, Sept. 2022, pp. 95-110.

52. Worsfold, B. L., and Moehle, J. P., “Moment Transfer at Column-Foundation Connections: Analytical Studies,” ACI Structural Journal, V. 120, No. 2, Mar. 2023, pp. 205-216.

53. Worsfold, B. L., and Moehle, J. P., “Shear-Reinforced Concrete Breakout Design Methodology for Moment Transfer at Column-Foundation Connections,” Engineering Structures, V. 283, 2023, p. 115783. doi: 10.1016/j.engstruct.2023.115783

54. Eligehausen, R.; Mallée, R.; and Silva, J. F., “Behaviour of Headed Studs, Undercut Anchors and Metal Expansion Anchors in Non-Cracked and Cracked Concrete,” Anchorage in Concrete Construction, 2012, pp. 65-162. doi: 10.1002/9783433601358.ch4


ALSO AVAILABLE IN: