Title:
Four Discussions from the September 2019 ACI Structural Journal
Author(s):
William L. Gamble; Jimmy Chandra and Susanto Teng; Emil de Souza Sánchez Filho; William L. Gamble
Publication:
Structural Journal
Volume:
117
Issue:
6
Appears on pages(s):
325-332
Keywords:
DOI:
Date:
11/1/2020
Abstract:
Disc. 116-S113/From the September 2019 ACI Structural Journal, p. 201 Reinforcement Limits for Reinforced Concrete Elements with High-Strength Steel. Paper by A. W. Puranam and S. Pujol
Disc. 116-S117/From the September 2019 ACI Structural Journal, p. 247 Novel Empirical Expression to Predict Shear Strength of Reinforced Concrete Walls Based on Particle Swarm. Paper by Hadi Baghi, Hani Baghi, and Sasan Siavashi
Disc. 116-S141/From the November 2019 ACI Structural Journal, p. 251 Torsional Behavior of Reinforced Concrete Beams with High-Strength Steel Bars. Paper by C. Kim, S. Kim, K.-H. Kim, D. Shin, M. Haroon, and J.-Y. Lee
Disc. 117-S04/From the January 2020 ACI Structural Journal, p. 43
Bond Behavior of 0.6 in. (15.2 mm) Prestressing Strand in Beltic Calcium Sulfoaluminate (BCSA) Cement Concrete. Paper by T. M. Bowser, C. D. Murray and R. W. Floyd