Title: Deployment of Composite Reinforcing

Author(s): Nolan, S., and Nanni, A

Publication: Concrete International

Volume: 39

Issue: 5

Appears on pages(s): 40-46

Keywords: fiber, reinforcement, standard, specification

DOI:

Date: 5/1/2017

Abstract:
Although fiber reinforced polymer (FRP) reinforcement has demonstrated great potential for improving the durability of concrete transportation infrastructure, adoption has been slowed by a lack of a unified strategy for deployment. Citing the successful introduction of prestressed concrete technology as a precedent, the authors call for development, publication, and sharing of standards and design guides for FRP applications.