Title:
Disc. 113-M15/From the March-April 2016 ACI Materials Journal, p. 151
Author(s):
Chao Jiang and Xiang-Lin Gu
Publication:
Materials Journal
Volume:
114
Issue:
1
Appears on pages(s):
185-186
Keywords:
DOI:
Date:
1/1/2017
Abstract:
Disc. 113-M15/From the March-April 2016 ACI Materials Journal, p. 151 Analysis of Compressive Strength Development and Carbonation Depth of High-Volume Fly Ash Cement Pastes. Paper by Xiao-Yong Wang and Ki-Bong Park