Title: Guide to Shotcrete

Author(s): Lars Balck

Publication: Concrete International

Volume: 39

Issue: 2

Appears on pages(s): 35-37

Keywords: gunite, specification, strength, testing

Date: 2/1/2017

Abstract:
This article is a reprint of a paper that originally appeared in the Summer 2016 issue of Shotcrete. It discusses updates to “Guide to Shotcrete (ACI 506R-16),” including new and expanded sections.




  