Title: A Safe Corrosion Solution for Potable Water Reservoirs

Author(s): Jessi Meyer, Jesús Orte Crespo, Josep Xavier Pujol, and Julie Holmquist

Publication: Concrete International

Volume: 39

Issue: 2

Appears on pages(s): 61-64

Keywords: concrete, admixture, carbonation, tank

Date: 2/1/2017

Abstract:
A new potable water reservoir was constructed in Tarragona, Spain. Based on past experiences, migrating corrosion inhibitors were selected to provide long-term protection against corrosion and help meet a 50-year design life. The admixtures had no apparent negative effects on the setting time or physical properties of the concrete.




  