Field Measurements of SCC Lateral Pressure—Toronto 2014
Author(s):
Gardner, N.J.; Keller, L.; Khayat, K.H.; Lange, D.A.; and Ahmed R. Omran
Publication:
Concrete International
Volume:
38
Issue:
6
Appears on pages(s):
42-50
Keywords:
thixotropy, reinforcement, vibration, hydrostatic
DOI:
Date:
6/1/2016
Abstract:
A large-scale experimental investigation to measure the form pressures exerted by self-consolidating concrete (SCC) was performed in Toronto, ON, Canada. The experimental program is described and measured lateral pressures are compared with values calculated using various predictive approaches available in the published literature. A key recommendation: Unless the stiffening characteristics of the SCC mixture are prequalified and verified by field measurements, formwork should be designed to resist full hydrostatic pressure.