Title:
SCC Under Pressure Research Program
Author(s):
Publication:
Concrete International
Volume:
37
Issue:
1
Appears on pages(s):
27-29
Keywords:
model, form, test, transducer
DOI:
Date:
1/1/2015
Abstract:
Various pressure models for self-consolidating concrete have been developed independently by researchers from Europe, the United States, and Canada. To help reconcile these models, RILEM Technical Committee 233-FPC, Form Pressure Generated by Fresh Concrete, was formed 5 years ago. The committee conducted full-scale wall tests two years ago in Stockholm, Sweden. As a continuation of this research, another testing program was carried out on tall column forms in Toronto, Canada, in 2014. This article provides a brief summary of the event.