Title:
Transforming Aggregate Constraints into Performance
Author(s):
G. Terry Harris Sr. and Aaron Lamb
Publication:
Concrete International
Volume:
48
Issue:
11
Appears on pages(s):
63-66
Keywords:
Manufactured sand; mid-range water reducer; rheology; circular economy; cement reduction; aggregate variability; slump retention; sustainable concrete.
DOI:
10.14359/51752128
Date:
11/1/2026
Abstract:
Aggregate variability is increasingly present in modern concrete production. Gap-graded aggregates, excess fines, and swelling clays disrupt cement dispersion and compromise workability, rheology, strength, and durability. This article highlights how challenging aggregates influence concrete behavior and spotlights Chryso®Quad, a range of mid-range water-reducing admixtures (MRWR) designed to mitigate these effects.