Treatment of Bar Group Breakout in ACI CODE-318-25—Part 1

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Treatment of Bar Group Breakout in ACI CODE-318-25—Part 1

Author(s): Benjamin L. Worsfold and Luis B. Fargier-Gabaldón

Publication: Concrete International

Volume: 48

Issue: 11

Appears on pages(s): 54-61

Keywords: Breakout strength, failure, anchor, concrete joints

DOI: 10.14359/51752127

Date: 11/1/2026

Abstract:
For many decades, standard detailing practice has relied on the assumption that the development length provides an adequate safeguard for transferring forces from reinforcement into concrete. Large-scale tests, however, show that under certain conditions, connections with groups of bars can exhibit a concrete breakout failure, even when the development length is provided. The findings were unexpected, as it had been assumed that the development length was sufficient to achieve bar yielding under tensile loads. In response, ACI CODE-318-25 introduced a new section (25.4.11) that requires checking the anchorage strength of groups of bars in tension, as well as a new section permitting the use of transverse reinforcement to strengthen the concrete breakout failure capacity (25.4.11.5). Part 1 of this article provides an overview of the background of these new provisions.

Related References:

1. ACI Committee 318, “Building Code for Structural Concrete—Code Requirements and Commentary (ACI CODE-318-25),” American Concrete Institute, Farmington Hills, MI, 2025, 702 pp.

2. Chicchi, R.; Varma, A.H.; Seo, J.; Bradt, T.; and McCarty, E., “Experimental Testing of Tension-Loaded Deformed Anchors in Concrete,” ACI Structural Journal, V. 117, No. 5, Sept. 2020, pp. 133-146. doi: 10.14359/51724670

3. ACI Committee 318, “Building Code Requirements for Structural Concrete and Commentary (ACI CODE-318-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

4. Klein, G.; Gleich, H.; Leistikow, R.; and Lucier, G., “Hanger Reinforcement for Corbels,” PCI Journal, V. 64, No. 6, Nov.-Dec. 2019, pp. 18-26. doi: 10.15554/pcij64.6-03

5. Cheng, M.-Y.; Chen, P.J., Chen, C.-H.; Worsfold, B.L.; Parra-Montesinos, G.J.; and Moehle, J.P., “Effect of Reinforcement Detailing on Cyclic Behavior of Reinforced Concrete Column-Footing Connections,” ACI Structural Journal, V. 122, No. 4, July 2025, pp. 19-34. doi: 10.14359/51746671

6. Worsfold, B.L.; Moehle, J.P.; and Silva, J.F., “Moment Transfer at Column-Foundation Connections: Physical Tests,” ACI Structural Journal, V. 119, No. 5, Sept. 2022, pp. 95-110. doi: 10.14359/51734799

7. Worsfold, B.L.; Karać, D.; and Moehle, J.P., “Shear-Reinforced Concrete Breakout Failure in Tension-Loaded Anchor Groups,” ACI Structural Journal, V. 122, No. 6, Sept. 2025, pp. 169-181. doi: 10.14359/51746720

8. Kusuhara, F., and Shiohara, H., “Seismic Performance of Reinforced Concrete Exterior Beam-Column Joint with Column-to-Beam Strength Ratio Equal or Near Unity,” Journal of Structural and Construction Engineering, Transactions of AIJ, Col. 78, No. 693, Nov. 2013, pp. 1939-1948. doi: 10.3130/aijs.78.1939

9. Worsfold, B.L., and Moehle, J.P., “Moment Transfer at Column-to-Footing Connections: Analytical Studies,” ACI Structural Journal, V. 120, No. 2, Mar. 2023, pp. 205-216. doi: 10.14359/51737146

10. Worsfold, B.L., and Moehle, J.P., “Shear-Reinforced Concrete Breakout Design Methodology for Moment Transfer at Column-Foundation Connections,” Engineering Structures, V. 283, May 2023, Article No. 115783. doi: 10.1016/j.engstruct.2023.115783

11. Fuchs, W.; Eligehausen, R.; and Breen, J.E., “Concrete Capacity Design (CCD) Approach for Fastening to Concrete,” ACI Structural Journal, V. 92, No. 1, Jan.-Feb. 1995, pp. 73-94. doi: 10.14359/1533

12. Pryor, S.; Montague, E.; Fischer, S.; Ding, F.; and Mochizuki, G., “Detailing for Increased Capacity of Tension-Only Steel Anchor Rods Embedded in Elevated Concrete Slabs,” 2016 SEAOC Convention, 2016.

13. Sharma, A.; Eligehausen, R.; and Asmus, J., “Comprehensive Experimental Investigations on Anchorages with Supplementary Reinforcement,” Proceedings, 3rd International Symposium on Connections between Steel and Concrete (ConSC 2017), Sept. 27-29, 2017, Stuttgart, Germany, pp. 242-252.

14. Lee, H.-J.; Yu, F.-C.; Lin, K.-C.; Wang, J.-C.; Worsfold, B. L.; and Silva, J. F., “High-Strength Headed Bars in Joints of Special Moment Frames under Cyclic Loading,” ACI Structural Journal, V. 121, No. 6, Nov. 2024, pp. 105-120. doi: 10.14359/51740866

15. Parra-Montesinos, G.J., and Zeuske, J., “Behavior of Exterior Beam-Column Connections with Headed Bars under Nonreversible Cyclic Loading,” ACI Structural Journal, V. 122, No. 5, Sept. 2025, pp. 71-81. doi: 10.14359/51746793