Abstract:
Traffic-bearing waterproofing membrane systems (traffic coatings) are commonly used in parking structures to provide protection against intrusion of moisture, chlorides, and other deleterious materials. They are typically impermeable and elastomeric, allowing the coating to accommodate movement of the concrete element that has been coated. This TechNote focuses on the most commonly used traffic coatings, comprising flexible polymer-based components. In addition to material selection considerations, surface preparation and quality assurance testing requirements should be specified based on structure and site considerations.
Related References:
ACI PRC-362.2-21—Parking Structure Structural Maintenance—Guide
ACI 515.3R-20—Guide for Assessment and Surface Preparation for Application of Protection Systems for Concrete
ASTM C1583/C1583M-13—Standard Test Method for Tensile Strength of Concrete Surfaces and the Bond Strength or Tensile Strength of Concrete Repair and Overlay Materials by Direct Tension (Pull-off Method)
ASTM D4263-83(2018)—Standard Test Method for Indicating Moisture in Concrete by the Plastic Sheet Method
ASTM F1869-16a—Standard Test Method for Measuring Moisture Vapor Emission Rate of Concrete Subfloor Using Anhydrous Calcium Chloride
ASTM F2170-19a—Standard Test Method for Determining Relative Humidity in Concrete Floor Slabs Using in situ Probes
ASTM F2659-10(2015)—Standard Guide for Preliminary Evaluation of Comparative Moisture Condition of Concrete, Gypsum Cement and Other Floor Slabs and Screeds Using a Non-Destructive Electronic Moisture Meter
ICRI 310.2R-2013—Selecting and Specifying Concrete Surface Preparation for Sealers, Coatings, Polymer Overlays, and Concrete Repair