Title:
CPC Position Statement #9: Differential Curing of Concrete Floors
Author(s):
Publication:
Concrete International
Volume:
48
Issue:
8
Appears on pages(s):
30
Keywords:
Curing, polished floors
DOI:
Date:
8/1/2026
Abstract:
Differential curing occurs when variations in curing methods, materials, or site conditions result in inconsistent moisture loss, hydration, or temperature across a concrete floor slab. This inconsistency can produce significant performance and appearance issues in both plain and polished concrete floors. This article highlights the causes and effects of differential curing, and best practices to achieve uniform curing.