Title: Efficient Arch Dam Construction

Author(s): Chongjiang Du

Publication: Concrete International

Volume: 48

Issue: 6

Appears on pages(s): 38-43

Keywords: Transverse contraction joint, arch dam, roller compacted concrete, MgO

DOI: 10.14359/51751761

Date: 6/1/2026

Abstract:
Over the past four decades, significant advances have been achieved in material science and construction technologies for the construction of dams. Among these, MgO concrete, rock-filled concrete, and roller-compacted concrete have been applied on an increasing trend in the construction of concrete dams. The application of these innovative materials and technologies in arch dam construction makes it possible to omit transverse and longitudinal contraction joints, which can speed up construction progress and reduce project costs. This paper discusses the design and construction features of arch dams constructed without contraction joints, highlighting the role of innovative materialsand associated construction methods.

Related References:

1. U.S. Bureau of Reclamation, Design of Arch Dams: Design Manual for Concrete Arch Dams, United States Government Printing Office, Denver, CO, 1977, 882 pp.

2. Li, C.M., “Long-Term Study on Autogenous Volume Expansion of MgO Concrete,” Journal of Hydroelectric Engineering, V. 18, No. 2, 1999, pp. 11-19. (in Chinese)

3. Du, C., “A Review of Magnesium Oxide in Concrete,” Concrete International, V. 27, No. 12, Dec. 2005, pp. 45-50.

4. Du, C., “Application of MgO Concrete in RCC Dams – A Review of the Status and Prospects for MgO Expansive Additives,” Concrete International, V. 41, No. 7, July 2019, pp. 41-48.

5. Mo, L.W.; Deng, M.; Tang, M.S.; and Al-Tabbaa, A., “MgO Expansive Cement and Concrete in China: Past, Present and Future,” Cement and Concrete Research, V. 57, Mar. 2014, pp. 1-12. doi: 10.1016/j.cemconres.2013.12.007

6. Guizhou Water Conservancy Hydropower Design and Research Institute, Research on Key Technology and Engineering Practice of Arch Dams Using MgO Concrete, China Water & Power Press, Beijing, 2016. (in Chinese)

7. Jin, F., and Huang, D.R., Rock-Filled Concrete Dam, first edition, Springer, Singapore, 2022, 340 pp. doi: 10.1007/978-981-16-8298-8

8. ICOLD Committee on Cemented Material Dams, Cemented Material Dam: Design and Practice—Rock-Filled Concrete Dam, Bulletin 190, International Commission on Large Dams (ICOLD), Paris, France, 2022, 111 pp.

9. Jin, F.; Huang, D.; Lino, M.; and Zhou, H., “A Brief Review of Rock-Filled Concrete Dams and Prospects for Next-Generation Concrete Dam Construction Technology,” Engineering, V. 32, Jan. 2024, pp. 99-105. doi: 10.1016/j.eng.2023.09.020

10. Jin, F., and Zhang, G.Y., “Rock-Filled Concrete Arch Dams with or Without Contraction Joints,” Proceedings of the 5th International Dam World Conference, Apr. 13-17, 2025, Lisbon, Portugal, V. 1, pp. 147-153.

11. Tao, Z., and Wan, K.H., “Chishui City Shaqian Reservoir Project Passed the Acceptance Inspection for Water Storage,” www.sohu.com/a/681535651_121106687, 2023. (in Chinese) (accessed May 4, 2026)

12. Du, C., “Prevention of Thermal Cracking in RCC Dams Using Magnesium Oxide (MgO) Concrete,” Proceedings of the 9th International Symposium on RCC Dams and CMDs, Dec. 4-5, 2023, Guangzhou, China, pp. 108-116

13. Zhang, G.X., and Zhang, Y., “Application of MgO Content to RCC Arch Dam,” New Progress on Roller Compacted Concrete Dams - Proceedings of the 5th International Symposium on Roller Compacted Concrete (RCC) Dams, J. Jia, L. Berga, G. Zhang, G. Chen, and C. Zheng, eds., Guiyang, China, 2007.

14. Zhu, B.F., “RCC Arch Dams: Temperature Control and Design of Joints,” International Water Power and Dam Construction, V. 55, No. 8, Aug. 2003, pp. 26-30.

15. Li, Z.W.; Qin, X.L.; Zhang, T.; and Zhang, Y.C., “RCC Construction Technology of Double - Curvature Arch Dam of Longtan Reservoir,” Proceedings of the 8th International Symposium on RCC Dams, Nov. 11-12, 2019, Kunming, China, pp. 382-388.

16. Chen, J., “New Breakthrough in Construction Technology for RCC Double-Curvature Arch Dams,” https://ynjtsl.com/artview/1967/118854.html, 2025. (in Chinese)

17. Du, C., and Stabel, B., “Innovative Technologies for Construction of RCC Arch Dams,” Proceedings of the 7th International Symposium on Roller Compacted Concrete (RCC) Dams, Sept. 24-25, 2015, Chengdu, China, pp. 444-460.