2025 Slag Cement in Sustainable Concrete Awards

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 2025 Slag Cement in Sustainable Concrete Awards

Author(s):

Publication: Concrete International

Volume: 48

Issue: 5

Appears on pages(s): 35-39

Keywords: Slag cement, embodied carbon, sustainability

DOI: 10.14359/51750690

Date: 5/1/2026

Abstract:
The Slag Cement Association (SCA) announced the recipients of the 2025 Slag Cement in Sustainable Concrete Awards during the ACI Concrete Convention – Spring 2026 in Rosemont/Chicago, IL, USA. Fourteen construction projects were selected to showcase the broad applications of slag cement and its impact on creating enduring and sustainable concrete.