Behavior of Basalt Fiber-Reinforced Polymer Bars after Exposure to High Temperatures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Basalt Fiber-Reinforced Polymer Bars after Exposure to High Temperatures

Author(s): Brandon Boles, Jahanzaib, and Shamim A. Sheikh

Publication: Structural Journal

Volume: 123

Issue: 4

Appears on pages(s): 103-118

Keywords: basalt fiber-reinforced polymer (BFRP); elevated temperature; glass fiber-reinforced polymer (GFRP); sustained load; tensile strength

DOI: 10.14359/51749408

Date: 7/1/2026

Abstract:
Research presented in this paper is part of a program investigating the durability of fiber-reinforced polymer reinforcement after exposure to a marine environment or elevated temperatures. This paper presents the results of an experimental study on the tensile behavior of basalt fiber-reinforced polymer (BFRP) bars after exposure to elevated temperatures under different heating protocols. Under the steady-state heating protocol, specimens were exposed to elevated temperatures up to 250°C (482°F) first and then subjected to monotonically increasing load until failure. In other testing protocols, specimens were exposed to a specific sustained stress level first, keeping deformation or load constant, and then heated until failure. Under these conditions, specimen stress levels varied from 39 to 91%. Results showed that different testing protocols yielded different results, and the criticality shifted between protocols depending on the stress level. Lastly, a direct comparison was made between BFRP and glass fiber-reinforced polymer (GFRP) bars tested under identical conditions. The direct comparison showed that thermal degradation of BFRP at higher stress levels was comparable with that of GFRP bars, whereas GFRP bars exhibited superior performance at lower stress levels.

Related References:

Abbood, I. S.; Odaa, S. A.; Hasan, K. F.; and Jasim, M. A., 2021, “Properties Evaluation of Fiber Reinforced Polymers and their Constituent Materials used in Structures: A Review,” Materials Today: Proceedings, V. 43, pp. 1003-1008. doi: 10.1016/j.matpr.2020.07.636

Ahmadi, J.; Shayanfar, M. A.; Ghanooni-Bagha, M.; Nasserasadi, K.; and Goharrokhi, A., 2020, “An Experimental Investigation into the Effect of Transverse Reinforcement Corrosion on Compressive Strength Reduction in Spirally Confined Concrete,” Iranian Journal of Science and Technology, Transactions of Civil Engineering, V. 44, No. 2, pp. 265-275. doi: 10.1007/s40996-020-00365-1

ASTM D2584-18, 2018, “Standard Test Method for Ignition Loss of Cured Reinforced Resins,” ASTM International, West Conshohocken, PA, 3 pp.

ASTM D7205/D7205M-21, 2021, “Standard Test Method for Tensile Properties of Fiber Reinforced Polymer Matrix Composite Bars,” ASTM International, West Conshohocken, PA, 13 pp.

ASTM E1356-23, 2023, “Standard Test Method for Assignment of the Glass Transition Temperatures by Differential Scanning Calorimetry,” ASTM International, West Conshohocken, PA, 4 pp.

Bush, E., and Lemmen, D. S., 2019, “Canada’s Changing Climate Report,” Government of Canada, Ottawa, ON, Canada.

Canadian Wood Council, 1996, “Fire Safety Design in Buildings: A Reference for Applying the National Building Code of Canada Fire Safety Requirements in Building Design,” Ottawa, ON, Canada.

CSA S806-12, 2021, “Design and Construction of Building Structures with Fibre-Reinforced Polymers,” CSA Group, Toronto, ON, Canada.

Hamad, R. J. A.; Johari, M. A. M.; and Haddad, R. H., 2017, “Mechanical Properties and Bond Characteristics of Different Fiber Reinforced Polymer Rebars at Elevated Temperatures,” Construction and Building Materials, V. 142, pp. 521-535. doi: 10.1016/j.conbuildmat.2017.03.113

Jahanzaib; Kharal, Z.; and Sheikh, S. A., 2021, “Behavior of Glass Fiber-Reinforced Polymer Bar Coupons Under Sustained Load and High Temperatures,” ACI Structural Journal, V. 118, No. 2, Mar., pp. 139-152.

Lin, S.; Zhao, Y. G.; Li, J.; and Lu, Z. H., 2021, “Confining Stress Path-Based Compressive Strength Model of Axially Loaded FRP-Confined Columns,” Journal of Composites for Construction, ASCE, V. 25, No. 1, pp. 1-14. doi: 10.1061/(ASCE)CC.1943-5614.0001090

United States Environmental Protection Agency, 2023, “Learn About Heat Island Effects,” Washington, DC, https://www.epa.gov/heatislands/learn-about-heat-islands. (last accessed June 5, 2026)

Wu, J.; Li, H.; and Xian, G., 2010, “Influence of Elevated Temperature on the Mechanical and Thermal Performance of BFRP Rebar,” CICE 2010 – The 5th International Conference on FRP Composites in Civil Engineering, pp. 69-72.


ALSO AVAILABLE IN:

Electronic Structural Journal