Curvilinearity Effect on Flexural and Shear Strengths of Vertically Curved Glass Fiber-Reinforced Polymer- Reinforced Concrete Flexural Members

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Curvilinearity Effect on Flexural and Shear Strengths of Vertically Curved Glass Fiber-Reinforced Polymer- Reinforced Concrete Flexural Members

Author(s): Seyed Mohammad Hosseini, Salaheldin Mousa, Hamdy M. Mohamed, and Brahim Benmokrane

Publication: Structural Journal

Volume: 122

Issue: 3

Appears on pages(s): 33-47

Keywords: critical shear crack theory (CSCT); curvilinear reinforced concrete (RC) members; design codes; experimental and analytical studies; flexural strength; glass fiber-reinforced polymer (GFRP) bars; Modified Compression Field Theory (MCFT); parametric studie

DOI: 10.14359/51745638

Date: 5/1/2025

Abstract:
The geometry of arched (vertically curved) reinforced concrete (RC) members contributes to the development of additional stresses, affecting their flexural and shear strengths. This aspect of curvilinear RC members reinforced with glass fiber-reinforced polymer (GFRP) bars has not been reported in the literature. In addition, no specific design recommendations consider the effect of curvilinearity on the flexural and shear strengths of curved GFRP-RC members. This study has performed pioneering work in developing models to predict the flexural and shear strengths of curvilinear GFRP-RC members, with a focus on precast concrete tunnel lining segments. Eleven full-scale curvilinear GFRPreinforced tunnel segment specimens were tested under bending load as the experimental database. Then, a model was developed for predicting the flexural strength of curvilinear GFRP-RC members. This was followed by the development of two shear-strength prediction models based on the Modified Compression Field Theory (MCFT) and critical shear crack theory (CSCT). After comparing the experimental and analytical results, a parametric study was performed to evaluate the effect of different parameters on the flexural and shear strengths of curvilinear GFRP-reinforced members. The results indicate that neglecting the curvilinearity effect led to a 17% overestimation of the flexural strength, while the proposed models could predict the flexural strength of the specimens accurately. The proposed models based on the MCFT—referred to as the semi-simplified Modified Compression Field Theory (SSMCFT) and the improved simplified Modified Compression Field Theory (ISMCFT)—predicted the shear strength of the specimens with 28% conservativeness. In addition, the modified critical shear crack theory (MCSCT) model was 10% conservative in predicting the shear strength of curvilinear GFRP-RC members.

Related References:

1. Gudonis, E.; Timinskas, E.; Gribniak, V.; Kaklauskas, G.; Arnautov, A. K.; and Tamulėnas, V., “FRP Reinforcement for Concrete Structures: State-of-the-Art Review of Application and Design,” Engineering Structures and Technologies, V. 5, No. 4, 2013, pp. 147-158. doi: 10.3846/2029882X.2014.889274

2. Alguhi, H., and Tomlinson, D., “One-Way Shear Strength of FRP–Reinforced Concrete Members Without Stirrups: Design Provision Review,” Journal of Composites for Construction, ASCE, V. 25, No. 3, June 2021, p. 04021016. doi: 10.1061/(ASCE)CC.1943-5614.0001125

3. El-Nemr, A.; Ahmed, E. A.; El-Safty, A.; and Benmokrane, B., “Evaluation of the Flexural Strength and Serviceability of Concrete Beams Reinforced with Different Types of GFRP Bars,” Engineering Structures, V. 173, Oct. 2018, pp. 606-619. doi: 10.1016/j.engstruct.2018.06.089

4. Kassem, C.; Farghaly, A. S.; and Benmokrane, B., “Evaluation of Flexural Behavior and Serviceability Performance of Concrete Beams Reinforced with FRP Bars,” Journal of Composites for Construction, ASCE, V. 15, No. 5, Oct. 2011, pp. 682-695. doi: 10.1061/(ASCE)CC.1943-5614.0000216

5. Khavaran, A., “Investigation of Shear-Critical One-Way Concrete Slabs Internally Reinforced with GFRP Bars,” PhD thesis, University of Toronto, Toronto, ON, Canada, 2019, 452 pp.

6. Mousa, S.; Mohamed, H. M.; Benmokrane, B.; and Nanni, A., “Flexural Behavior of Long-Span Square Reinforced Concrete Members with Uniformly Distributed Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 117, No. 4, July 2020, pp. 209-222.

7. Protchenko, K.; Leśniak, P.; Szmigiera, E.; and Urbański, M., “New Model for Analytical Predictions on the Bending Capacity of Concrete Elements Reinforced with FRP Bars,” Materials, V. 14, No. 3, Feb. 2021, Article No. 693. doi: 10.3390/ma14030693

8. Thériault, M., and Benmokrane, B., “Effects of FRP Reinforcement Ratio and Concrete Strength on Flexural Behavior of Concrete Beams,” Journal of Composites for Construction, ASCE, V. 2, No. 1, Feb. 1998, pp. 7-16. doi: 10.1061/(ASCE)1090-0268(1998)2:1(7)

9. ACI Committee 440, “Building Code Requirements for Structural Concrete Reinforced with Glass Fiber-Reinforced Polymer (GFRP) Bars—Code and Commentary (ACI CODE-440.11-22),” American Concrete Institute, Farmington Hills, MI, 2022, 260 pp.

10. CSA S6:19 (R2024), “Canadian Highway Bridge Design Code (Reaffirmed in 2024),” CSA Group, Toronto, ON, Canada, 2019, 1182 pp.

11. CSA S806:12 (R2021), “Design and Construction of Building Structures with Fibre-Reinforced Polymers (Reaffirmed in 2021),” CSA Group, Toronto, ON, Canada, 2012, 201 pp.

12. AASHTO, “AASHTO LRFD Bridge Design Guide Specifications for GFRP-Reinforced Concrete,” second edition, American Association of State Highway and Transportation Officials, Washington, DC, 2018, 121 pp.

13. Adam, M. A.; Said, M.; Mahmoud, A. A.; and Shanour, A. S., “Analytical and Experimental Flexural Behavior of Concrete Beams Reinforced with Glass Fiber Reinforced Polymers Bars,” Construction and Building Materials, V. 84, June 2015, pp. 354-366. doi: 10.1016/j.conbuildmat.2015.03.057

14. Ali, A. H.; Mohamed, H. M.; Chalioris, C. E.; and Deifalla, A., “Evaluating the Shear Design Equations of FRP-Reinforced Concrete Beams without Shear Reinforcement,” Engineering Structures, V. 235, May 2021, Article No. 112017. doi: 10.1016/j.engstruct.2021.112017

15. Razaqpur, A. G., and Spadea, S., “Shear Strength of FRP Reinforced Concrete Members with Stirrups,” Journal of Composites for Construction, ASCE, V. 19, No. 1, Feb. 2015, p. 04014025. doi: 10.1061/(ASCE)CC.1943-5614.0000483

16. Bentz, E. C.; Vecchio, F. J.; and Collins, M. P., “Simplified Modified Compression Field Theory for Calculating Shear Strength of Reinforced Concrete Elements,” ACI Structural Journal, V. 103, No. 4, July-Aug. 2006, pp. 614-624.

17. Sadeghian, V., and Vecchio, F., “The Modified Compression Field Theory: Then and Now,” Shear in Structural Concrete, SP-328, D. Mitchell and A. Belarbi, eds., American Concrete Institute, Farmington Hills, MI, 2018, pp. 3.1-3.20.

18. Hoult, N. A.; Sherwood, E. G.; Bentz, E. C.; and Collins, M. P., “Does the Use of FRP Reinforcement Change the One-Way Shear Behavior of Reinforced Concrete Slabs?” Journal of Composites for Construction, ASCE, V. 12, No. 2, Apr. 2008, pp. 125-133. doi: 10.1061/(ASCE)1090-0268(2008)12:2(125)

19. Muttoni, A., and Fernández Ruiz, M., “Shear Strength of Members without Transverse Reinforcement as Function of Critical Shear Crack Width,” ACI Structural Journal, V. 105, No. 2, Mar.-Apr. 2008, pp. 163-172.

20. Cavagnis, F.; Fernández Ruiz, M.; and Muttoni, A., “Shear Failures in Reinforced Concrete Members without Transverse Reinforcement: An Analysis of the Critical Shear Crack Development on the Basis of Test Results,” Engineering Structures, V. 103, Nov. 2015, pp. 157-173. doi: 10.1016/j.engstruct.2015.09.015

21. Cavagnis, F.; Fernández Ruiz, M.; and Muttoni, A., “A Mechanical Model for Failures in Shear of Members without Transverse Reinforcement Based on Development of a Critical Shear Crack,” Engineering Structures, V. 157, Feb. 2018, pp. 300-315. doi: 10.1016/j.engstruct.2017.12.004

22. Cavagnis, F.; Simões, J. T.; Fernández Ruiz, M.; and Muttoni, A., “Shear Strength of Members without Transverse Reinforcement Based on Development of Critical Shear Crack,” ACI Structural Journal, V. 117, No. 1, Jan. 2020, pp. 103-118. doi: 10.14359/51718012

23. Fernández Ruiz, M.; Muttoni, A.; and Sagaseta, J., “Shear Strength of Concrete Members without Transverse Reinforcement: A Mechanical Approach to Consistently Account for Size and Strain Effects,” Engineering Structures, V. 99, Sept. 2015, pp. 360-372. doi: 10.1016/j.engstruct.2015.05.007

24. Caratelli, A.; Meda, A.; Rinaldi, Z.; and Spagnuolo, S., “Precast Tunnel Segments with GFRP Reinforcement,” Tunnelling and Underground Space Technology, V. 60, Nov. 2016, pp. 10-20. doi: 10.1016/j.tust.2016.07.011

25. Caratelli, A.; Meda, A.; Rinaldi, Z.; Spagnuolo, S.; and Maddaluno, G., “Optimization of GFRP Reinforcement in Precast Segments for Metro Tunnel Lining,” Composite Structures, V. 181, Dec. 2017, pp. 336-346. doi: 10.1016/j.compstruct.2017.08.083

26. ACI Committee 533, “Guide for Precast Concrete Tunnel Segments (ACI 533.5R-20),” American Concrete Institute, Farmington Hills, MI, 2020, 84 pp.

27. Campana, S.; Fernández Ruiz, M.; and Muttoni, A., “Shear Strength of Arch-Shaped Members without Transverse Reinforcement,” ACI Structural Journal, V. 111, No. 3, May-June 2014, pp. 573-582. doi: 10.14359/51686574

28. Fernández Ruiz, M.; Plumey, S., and Muttoni, A., “Interaction between Bond and Deviation Forces in Spalling Failures of Arch-Shaped Members without Transverse Reinforcement,” ACI Structural Journal, V. 107, No. 3, May-June 2010, pp. 346-354.

29. ASTM D7205/D7205M-21, “Standard Test Method for Tensile Properties of Fiber Reinforced Polymer Matrix Composite Bars,” ASTM International, West Conshohocken, PA, 2021, 13 pp.

30. ASTM C39/C39M-21, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2021, 8 pp.

31. ASTM C1609/C1609M-19, “Standard Test Method for Flexural Performance of Fiber-Reinforced Concrete (Using Beam With Third-Point Loading),” ASTM International, West Conshohocken, PA, 2019, 9 pp.

32. Hussein, A., and Marzouk, H., “Behavior of High-Strength Concrete under Biaxial Stresses,” ACI Materials Journal, V. 97, No. 1, Jan.-Feb. 2000, pp. 27-36.

33. Kupfer, H.; Hilsdorf, H. K., and Rusch, H., “Behavior of Concrete Under Biaxial Stresses,” ACI Journal Proceedings, V. 66, No. 8, Aug. 1969, pp. 656-666.

34. Nelissen, L. J. M., “Biaxial Testing of Normal Concrete,” HERON, V. 18, No. 1, 1972, pp. 1-90.

35. Buyukozturk, O.; Nilson, A. H.; and Slate, F. O., “Stress-Strain Response and Fracture of a Concrete Model in Biaxial Loading,” ACI Journal Proceedings, V. 68, No. 8, Aug. 1971, pp. 590-599.

36. Tasuji, M. E.; Slate, F. O.; and Nilson, A. H., “Stress-Strain Response and Fracture of Concrete in Biaxial Loading,” ACI Journal Proceedings, V. 75, No. 7, July 1978, pp. 306-312.

37. Darwin, D.; Dolan, C. W.; and Nilson, A. H., Design of Concrete Structures, 15th edition, McGraw-Hill Education, New York, NY, 2016, 800 pp.

38. Chang, K., and Seo, D., “Behavior of One-Way Concrete Slabs Reinforced with GFRP Bars,” Journal of Asian Architecture and Building Engineering, V. 11, No. 2, 2012, pp. 351-358. doi: 10.3130/jaabe.11.351

39. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

40. Zheng, W.; Kwan, A. K. H.; and Lee, P. K. K., “Direct Tension Test of Concrete,” ACI Materials Journal, V. 98, No. 1, Jan.-Feb. 2001, pp. 63-71.

41. Todeschini, C. E.; Bianchini, A. C., and Kesler, C. E., “Behavior of Concrete Columns Reinforced with High Strength Steels,” ACI Journal Proceedings, V. 61, No. 6, June 1964, pp. 701-716.

42. Nader Tehrani, B.; Mostofinejad, D.; and Hosseini, S. M., “Experimental and Analytical Study on Flexural Strengthening of RC Beams via Prestressed EBROG CFRP Plates,” Engineering Structures, V. 197, Oct. 2019, Article No. 109395. doi: 10.1016/j.engstruct.2019.109395

43. ACI Committee 363, “Report on High-Strength Concrete (ACI 363R-10),” American Concrete Institute, Farmington Hills, MI, 2010, 65 pp.

44. Ozbakkaloglu, T., and Saatcioglu, M., “Rectangular Stress Block for High-Strength Concrete,” ACI Structural Journal, V. 101, No. 4, July-Aug. 2004, pp. 475-483.

45. Collins, M. P., and Mitchell, D., Prestressed Concrete Structures, Prentice Hall, Englewood Cliffs, NJ, 1991, 766 pp.

46. Swaddiwudhipong, S., and Seow, P. E. C., “Modelling of Steel Fiber-Reinforced Concrete under Multi-Axial Loads,” Cement and Concrete Research, V. 36, No. 7, July 2006, pp. 1354-1361.

47. ACI Committee 544, “Guide to Design with Fiber-Reinforced Concrete (ACI 544.4R-18),” American Concrete Institute, Farmington Hills, MI, 2018, 44 pp.

48. Vecchio, F. J., and Collins, M. P., “The Modified Compression-Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr. 1986, pp. 219-231.

49. Johnson, D. T. C., “Investigation of Glass Fibre Reinforced Polymer (GFRP) Bars as Internal Reinforcement for Concrete Structures,” PhD thesis, University of Toronto, Toronto, ON, Canada, 2014, 453 pp.

50. El-Sayed, A. K.; El-Salakawy, E. F.; and Benmokrane, B., “Shear Capacity of High-Strength Concrete Beams Reinforced with FRP Bars,” ACI Structural Journal, V. 103, No. 3, May-June 2006, pp. 383-389.

51. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

52. Arnau, O., and Molins, C., “Three Dimensional Structural Response of Segmental Tunnel Linings,” Engineering Structures, V. 44, Nov. 2012, pp. 210-221. doi: 10.1016/j.engstruct.2012.06.001


ALSO AVAILABLE IN:

Electronic Structural Journal