Title: Moving Away from Carbon Neutrality Turmoil

Author(s): Koji Sakai and Takeju Matsuka

Publication: Concrete International

Volume: 46

Issue: 11

Appears on pages(s): 58-60

Keywords: concrete, cement, agreement, fossil fuels

DOI:

Date: 11/1/2024

Abstract:
Carbon neutrality has been set by the industrial world as a goal to be reached by 2050. In this article, the authors attempt to provide a clear vision of the nature of the turmoil concerning carbon neutrality in cement and concrete industries and discuss measures toward this historic transformation.




  