Title: Pumping Up Profits

Author(s): Tripp Farrell

Publication: Concrete International

Volume: 42

Issue: 12

Appears on pages(s): 45-48

Keywords: shotcrete, wet-mix, dry-mix, pumps

Date: 12/1/2020

Abstract:
This article provides guidance on concrete pumps for contractors looking to expand their services into shotcrete. It discusses the use of rotary gunite machines for dry-mix shotcrete and four pump types that are available for delivering wet-mix concrete: swing tube piston, squeeze tube (peristaltic), rotor stator (progressive cavity), and hydraulic ball valve pumps.




  