Title:
Guide for Evaluation of Concrete Structures Prior to Rehabilitation (ACI 364.1R)
Author(s):
ACI Committee 364
Publication:
Materials Journal
Volume:
90
Issue:
5
Appears on pages(s):
479-498
Keywords:
buildings; concrete; condition survey; evaluation; field observation; historic structures; nondestructive evaluation; rehabilitation; sampling; service history; testing; Materials Research
DOI:
10.14359/3883
Date:
9/1/1993
Abstract:
This report presents the guidelines and general procedures that may be used for evaluation of concrete structures prior to rehabilitation. Among the subjects covered are: preliminary investigation; detailed investigation; documentation; field inspection and condition survey; sampling and material testing; evaluation; and final report. Seismic evaluation is considered beyond the scope of this report.