Designing Prestressed Barrier Cables

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Designing Prestressed Barrier Cables

Author(s): Hoshang Presswalla

Publication: Concrete International

Volume: 11

Issue: 5

Appears on pages(s): 67-73

Keywords: barriers; deflection; guard rails; measurement; tension; parking facilities; prestressing steels; structural design; Design

Date: 5/1/1989

Abstract:
Presents two rational methods of determining the initial prestress force as well as the additional cable tension for barrier cables in parking structures due to prescribed vehicular accident loads. One method is based on code requirements and the other on energy concepts.