ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Admixtures on Performance and Economics of Recycled Aggregate Concrete

Author(s): V. Corinaldesi and G. Moriconi

Publication: Symposium Paper

Volume: 199

Issue:

Appears on pages(s): 869-884

Keywords: building rubble; chemical admixture; concrete costs; envi-ronmental advantages; mineral admixture; recycled aggregate con-crete

DOI: 10.14359/10553

Date: 6/1/2001

Abstract:
Concrete specimens were manufactured by completely replacing natural aggregates with recycled aggregates from a crushing plant in which rubble from building demolition was ground. Various concrete was prepared by using silica fume or fly ash as a partial fine aggregate replacement and by using an acrylic polymer based superplasticizer to achieve the prefixed workability. Three types of recycled aggregate concrete were manufactured with the same water/cement (0.40) and the same fresh workability (fluid consistency). A reference concrete was also prepared by using natural aggregates with the same particle size distribution as the recycled aggregate, and having a water/cement of 0.56 and a similar fluid consistency. The results obtained show that because of mineral addition and W/C reduction, recycled aggregates can be used instead of natural aggregates since concretes with similar compressive strength can be obtained. The use of the recycled aggregates with fly ash replacements also has significant cost and environmental advantages over ordinary concrete.