This Specification describes the work of repairing defects in hardened portland-cement concrete with an epoxy mortar. Included are controls for epoxy resin system labeling, storage, handling, surface evaluation and preparation, mixing and application, inspection, quality control, and testing.
The Online Collection contains all new ACI Standards & Practices. The most recently added included:
PRC-555-26: Use of Recycled Concrete Aggregate in Portland Cement Concrete—Guide
CODE-318-25: Building Code for Structural Concrete—Code Requirements and Commentary (CODE-318-25)—Spanish
PRC-234-26: Use of Silica Fume in Concrete—Guide
PRC-325.12-26: Design of Jointed Concrete Pavements for Streets and Local Roads—Guide
PRC-238.1-26: Measurements of Workability and Rheology of Fresh Concrete—Report
RAP Bulletin 15-26: Structural Strengthening Using Fiber-Reinforced Polymer (FRP)