318.2M-19 Building Code Requirements for Concrete Thin Shells and Commentary (SI Units)

Abstract:

This document governs the design of thin shell concrete structures. Where required for design of thin shell concrete structures, provisions of ACI 318 are to be used to complement the provisions of this Code.