222R-19 Guide to Protection of Reinforcing Steel in Concrete against Corrosion

Abstract:

This guide reviews the most recent developments of metal corrosion, specifically reinforcing steel, in concrete. Individual chapters are devoted to corrosion of metals in concrete, protective measures for new concrete construction, procedures for identifying corrosive environments, active corrosion in concrete, and remedial measures.