ACI 123 Student Poster Session

Monday, October 24, 2022  10:30 AM - 12:00 PM, H-Marsalis Hall

The ACI 123 Concrete Research Poster Session compliments the existing Research in Progress and Open Topic Presentation sessions and provides further opportunity for the presentation of original, unpublished results from ongoing research projects and leading-edge concrete technology throughout the world.
Learning Objectives:
(1) Recognize ongoing concrete research projects from a wide range of research topics;
(2) Discuss recent techniques, research methods, and procedures related to structural and material aspects of concrete research one-on-one with the authors;
(3) Describe emerging ideas in concrete research;
(4) Summarize recent technical information related to concrete structures and materials research.

This session has been AIA/ICC approved for 2 CEU/PDH credits.


Rheological Properties of 3D Printable Concrete with Cellulose Microfibers: Effect of Accelerators

Presented By: Eunsan Cho
Affiliation: Ulsan National Institute of Science and Technology
Description:


Rheological Characterization of Cement Slurries with High Magnetic Particle Concentrations under Low Magnetic Field Strengths

Presented By: Sriramya Nair
Affiliation: Cornell University
Description:


Hybrid Ultra-High-Performance Concrete/Conventional Concrete Prestressed Girders

Presented By: Jacob Choate
Affiliation: University of Oklahoma
Description:


Strength and Drying Shrinkage Performance of Geopolymer Concretes

Presented By: Sourav Thapa
Affiliation: Clarkson University
Description:


Monitoring Strength Development of Concrete Under Different Curing Conditions Using Diffuse Ultrasound

Presented By: Geetanjali Chandam
Affiliation: Ulsan National Institute of Science & Technology
Description:


Supplementary and Alternative Cementitious Materials Under Extreme Environments

Presented By: Sriramya Nair
Affiliation: Cornell University
Description:


Distributed Strain Behavior of Two-Way Slabs Produced with Low Carbon Concrete

Presented By: Peace Ikpotokin
Affiliation: York University
Description:


Experiment on Noncontact Lap-Splices of #6 Gr. 80 Reinforcing Bars

Presented By: So-Hyun Mun
Affiliation: Incheon National University
Description:


Increasing Seismic Resilience of School Infrastructure of Mexico City Through a Seismic Assessment and Rehabilitation Plan

Presented By: Gianella Ronquillo
Affiliation: National Autonomous University of Mexico
Description:


Quantifying Compactability of Roller-Compacted Concrete with Gyratory Compactor

Presented By: Jordan Ouellet
Affiliation: University of Illinois Urbana-Champaign
Description:


Long-Term Performance of Soy Methyl Ester-Polystyrene (SM-PS) as Concrete Surface Protectant Exposed to Accelerated Laboratory Aging Conditions

Presented By: Mohammad Khaneghahi
Affiliation: Drexel University
Description:


Evaluation of Seamless Bridge-Pavement Systems

Presented By: Xiaoyi Chen
Affiliation: University of Texas Austin
Description:


Self-sensing Capacity of Cementless UHPFRC in Tension

Presented By: MinChang Kang
Affiliation: Ulsan National Institute of Science and Technology
Description:


Effect of pH on the Hydration Kinetics and Early Age Properties of Clinoptilolite Zeolite-Based Cementitious Materials

Presented By: M. Shariful Islam
Affiliation: Tennessee Tech University
Description:


Utilization of Coal Bottom Ash for an Alkaline Solution of Metakaolin-Based Geopolymer by Minimizing Bubble Generation

Presented By: Ju Suhawn
Affiliation: Ulsan National Institute of Science & Technology
Description:


Unlock CO2 Sequestration Potential of Concrete through a Bio-Regulated Carbonation Process

Presented By: Xiaodong Wang
Affiliation: The University of Alabama
Description:


Microencapsulation of Biobased Phase Change Materials with Silica Coated Inorganic Microcapsule for Thermal Energy Storage

Presented By: Abdulmalik Ismail
Affiliation: University of Alabama
Description:


Contaminants on Ground Glass Pozzolan and the Effects on Pozzolan Performance in Mortar

Presented By: Mary Christiansen
Affiliation: University of Minnesota Duluth
Description:


Influence of Supplementary Cementitious Materials on the Drying Shrinkage and Alkali-Silica Reaction of Concrete

Presented By: Abu Sayed Mohammad Akid
Affiliation: Arkansas State University
Description:

Upper Level Sponsors

Ash Grove
Baker
Conseal
Controls Group
Euclid Chemical
GCP
Master Builders
PoreShield
PS=0
ACI Northeast Texas Chapter

Please enter this 5 digit unlock code on the web page.