Title: Meeting Extreme Demands

Author(s): Michael H. Weber

Publication: Concrete International

Volume: 35

Issue: 5

Appears on pages(s): 52-54

Keywords: acid, temperature, durability, corrosion, strength

Date: 5/1/2013

Abstract:
Concrete surfaces in industrial facilities may be exposed to a wide range of extreme environments, including strong acids or high temperatures. Ceratech’s activated fly ash cement concrete systems, KEMROK™ and FIREROK™, show remarkable durability in such environments.