Title: Products & Practice Spotlight: Innovative Precast Solutions for School Buildings

Author(s):

Publication: Concrete International

Volume: 34

Issue: 10

Appears on pages(s): 51-53

Keywords:

Date: 10/1/2012

Abstract:
Insulated sandwich panels provide far more than thermal efficiency