Title: Sustainable Design of Buildings by Post-Tensioning Concrete

Author(s): Pawan R. Gupta and C. Nicholas Watry

Publication: Concrete International

Volume: 34

Issue: 10

Appears on pages(s): 42-47

Keywords:

Date: 10/1/2012

Abstract:
Case study illustrates how system can minimize cost and environmental impact