Title: 440.6-08 Specification for Carbon and Glass Fiber-Reinforced Polymer Bar Materials for Concrete Reinforcement
Author: ACI Committee 440
Year of Publication: 2008
Number of Pages: 6
This document is: Active
Nonmember Price: $30.50
ACI Member Price: $19.00
Order Code: 440608
Abstract: This Material Specification covers provisions governing testing, evaluation, and acceptance of carbon and glass fiber-reinforced polymer (FRP) bars used as reinforcement for concrete. Keywords: carbon fiber; concrete; concrete construction; FRP reinforced concrete; fiber-reinforced polymer reinforcement; glass fiber; specification.
Contents: CONTENTS Section 1—Scope, p. 440.6-2 Section 2—Referenced documents, p. 440.6-2 Section 3—Terminology, p. 440.6-2 Section 4—Classification, p. 440.6-2 Section 5—Ordering information, p. 440.6-3 Section 6—Materials and manufacture, p. 440.6-3 Sections 7—Physical properties, p. 440.6-3 Section 8—Mechanical properties, p. 440.6-4 Section 9—Durability properties, p. 440.6-4 Section 10—Other requirements, p. 440.6-5 Section 11—Sampling, p. 440.6-5 Section 12—Rejection, p. 440.6-5 Section 13—Product certification, p. 440.6-5 Section 14—Markings, p. 440.6-6
|