ACI - American Concrete Institute
About ACI Bookstore & Publications Certification Chapters Committees Conventions & Events Education International Membership Students Technical
  ACI Bookstore
 
Not Logged in - ATTENTION MEMBERS: You will not receive member prices until you log in
 
 
 
cart.gif (1759 bytes)
Delete Item    ITEM: RPRINTP-12247
ci2702abou-zied.pdf
ELEC
$25.00 .... $25.00

Delete Item    ITEM: RPRINTP-15514
ci0801wilson.pdf
ELEC
$25.00 .... $25.00

Delete Item    ITEM: RPRINTP-9400
ci2603amick.pdf
ELEC
$25.00 .... $25.00

Delete Item    ITEM: RPRINTP-8089
ci2110rizkalla.pdf
ELEC
$25.00 .... $25.00

Delete Item    ITEM: RPRINTP-11755
ci2612whittier.pdf
ELEC
$25.00 .... $25.00

TOTAL: $125.00
Clear Cart

Check Out

 
Instructions:

Click delete to delete item.

Member Prices
To receive member prices on the Bookstore you must be registered. If you have already registered and are not receiving member prices, you may need to log-in.

Resume Downloads
If for some reason you lose your connection while downloading a document you can resume the download by clicking on this link.

PDF Portable Document Format
All documents available for download are stored in PDF format and require a PDF reader to view them. You may download the free Adobe Acrobat Reader at the following link.  

 

 

Download an electronic version to my computer.  

This item is also available as hard copy.



 
You may also be interested in these items:
SP-264 Serviceability of Concrete Members Reinforced with Internal/External FRP Reinforcement CD-ROM
SP-257: FRP Stay-In-Place Forms for Concrete Structures CD-ROM
440.2R-08 Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures
440.6M-08 Metric Specification for Carbon & Glass Fiber-Reinforced Polymer Bar Materials for Conc Reinforcement
440.6-08 Specification for Carbon and Glass Fiber-Reinforced Polymer Bar Materials for Concrete Reinforcement
440.5M-08 Metric Specification for Construction with Fiber-Reinforced Polymer (FRP) Reinforcing Bars
440.5-08 Specification for Construction with Fiber-Reinforced Polymer Reinforcing Bars
421.1R-08 - Guide to Shear Reinforcement for Slabs
440R-07 Report on Fiber-Reinforced Polymer (FRP) Reinforcement for Concrete Structures
SP-245CD Case Histories and Use of FRP for Prestressing Applications
440.1R-06: Guide for the Design and Construction of Structural Concrete Reinforced with FRP Bars
SP-230: 7th International Symposium on Fiber-Reinforced (FRP) Polymer Reinforcement for Concrete Structures
440.4R-04: Prestressing Concrete Structures with FRP Tendons

Title: 440.3R-04: Guide Test Methods for Fiber-Reinforced Polymers (FRPs) for Reinforcing or Strengthening Concrete Structures

Author: ACI Committee 440
Year of Publication: 2004
Number of Pages: 40
This document is: Active
Nonmember Price: $70.50
ACI Member Price: $42.00
Order Code: 440304

Abstract: FRP reinforcing bars and laminates offer advantages over steel reinforcement in that FRP is noncorrosivedoes not corrode and is nonconductive. FRP reinforcing bars, grids, and tendons are being used for nonprestressed and prestressed concrete structures. FRP laminates are being used as external reinforcement for strengthening of existing concrete and masonry structures. Due to differences in the physical and mechanical behavior of FRP materials compared to steel, unique test methods for FRP bars and laminates are required.

This document provides model test methods for the short-term and long-term mechanical, thermo-mechanical, and durability testing of FRP bars and laminates. It is anticipated that these model test methods may be considered, modified, and adopted, either in whole or in part, by a U.S.national standards-writing agency such as ASTM International or AASHTO. The publication of these test methods by ACI Committee 440 is an effort to aid in this adoption.

The recommended test methods are based on the knowledge gained from research results and literature worldwide. Many of the proposed test methods for reinforcing rods are based on those found in “Recommendation for Design and Construction of Concrete Structures using Continuous Fiber Reinforcing Materials” published in 1997 by the Japan Society for Civil Engineers (JSCE). The JSCE test methods have been modified extensively to add details and to adapt the test methods to U.S. practice.

Keywords: anchorage; bond; concrete; coupler; creep; fatigue; fiber-reinforced

polymers (FRP); modulus of elasticity; reinforced concrete;

shear; splice; stirrup; strength; tendon.

Contents: CONTENTS

Part 1—General

1.1—Introduction

1.2—Scope

1.3—Existing ASTM test methods

1.4—Definitions

1.5—Notation

Part 2—Test methods for FRP bars for concrete structures

B.1—Test method for cross-sectional properties of FRP bars

B.2—Test method for longitudinal tensile properties of FRP bars

B.3—Test method for bond strength of FRP bars by pullout testing

B.4—Test method for transverse shear strength of FRP bars

B.5—Test method for strength of FRP bent bars and stirrups at bend locations

B.6—Accelerated test method for alkali resistance of FRP bars

B.7—Test method for tensile fatigue of FRP bars

B.8—Test method for creep rupture of FRP bars

B.9—Test method for long-term relaxation of FRP bars

B.10—Test method for performance of anchorages of FRP bars

B.11—Test method for tensile properties of deflected FRP bars

B.12—Test method for determining the effect of corner radius on tensile strength of FRP bars

Part 3—Test methods for FRP laminates for concrete and masonry

L.1—Test method for direct tension pull-off test

L.2—Test method for tension test of flat specimen

L.3—Test method for overlap splice tension test

References

R.1—Guides and related standards

R.2—Conference proceedings

R.3—Individual papers, reports, and theses

Appendix A—Anchor for testing FRP bars under monotonic, sustained, and cyclic tension,

Appendix B—Methods for calculating tensile properties of flat specimen



Download an electronic version to my computer.  