SP-254: Nanotechnology of Concrete: Recent Developments and Future Perspectives
Year of Publication: 2008
Number of Pages: 164
This document is: Active
Nonmember Price: $79.50
ACI Member Price: $48.00
Order Code: SP254
ISBN: 9780870312991
Category: Materials
Formats: Hard Copy

Ship a hard copy of this item to me.

Quantity:    

Abstract: Editors: K. Sobolev, S.P. Shah

Sponsored by ACI Committee 236

This volume consists of ten papers that were presented at a technical session, sponsored by ACI Committee 236, Materials of Science of Concrete, at the ACI Fall 2006 Convention in Denver, CO. Papers include “ Nanotechnology in Construction: A Roadmap for Development”, “ Nanotechnology and Concrete: Research Opportunities”, “Molecular Engineering of the Cohesion in Neat and Hybrid Cement Hydrates”, and “Use of Atomic Force Microscopy and Nanoindentation for Characterization of Cementitious Materials at the Nanoscale”.

Note: The individual papers are also available as .pdf downloads. Please click on the following link to view the papers available, or call 248.848.3800 to order.

VIEW THE PAPERS

Contents: SP-254—1

Nanotechnology in Construction: A Roadmap for Development

by P.J.M. Bartos

SP-254—2

Nanotechnology and Concrete: Research Oppurtunities

by P. Balaguru and K. Chong

SP-254—3

Molecular Engineering of the Cohesion in Neat and Hybrid Cement Hydrates

by A. Gmira, J. Minet, A. Francischini, N. Lequeux, R.J.-M. Pellenq, and H. Van Damme

SP-254—4

Use of Atomic Force Microscopy and Nanoindentation for Characterization of

Cemetitious Materials at the Nanoscale.

by P. Mondal, S.P. Shah, and L.D. Marks

SP-254—5

Utilization of Micro-Indentation Technique to Determine the Micromechanical

Properties of ITZ in Cementitious Materials

by M. Sonebi

SP-254—6

The Role of Nanotechnology for the Development of Sustainable Concrete

by H.J.H. (Jos) Brouwers

SP-254—7

Nanomaterials and Nanotechnology for High-Performance Cement Composites

by K. Sobolev, I. Flores, R. Hermosillo, and L.M. Torres-Martínez

SP-254—8

Development of a High-Density Cementitious Rock-Matching Grout using

Nano-Particles

by B.H. Green

SP-254—9

Effect of Moisture on Electrical Properties of Carbon Black-Filled

Cement Composites

by H. Li, H. Xiao, and J. Ou

SP-254—10

Macro-Defect-Free Materials with Controlled Moisture Resistance

by M. Drábik, L. Gáliková, S. Balkovic, and R.C.T. Slade