549.3R-09 Report on Glass Fiber-Reinforced Concrete Premix
Author: Committee 549
Year of Publication: 2009
Number of Pages: 24
This document is: Active
Nonmember Price: $56.50
ACI Member Price: $34.00
Order Code: 549309
ISBN: 9780870313547
Category: Ferrocement
Formats: Hard Copy or PDF

Note: You cannot mix hard copy orders with electronic downloads.

Ship a hard copy of this item to me.

Quantity:    


Download an electronic version to my computer.  

Abstract: Glass fiber-reinforced concrete premix technology is becoming increasingly popular worldwide for manufacture of precast concrete products used in industrial, architectural, civil engineering, and construction applications. Glass fiber-reinforced concrete premix products provide a useful balance of properties such as strength, toughness, durability, moisture resistance, dimensional stability, fire resistance, and aesthetics. This report summarizes the current knowledge of materials, manufacturing methods, engineering properties, and applications of glass fiber-reinforced concrete premix.

Keywords: cement-based composites; cement boards; cement panels; composite materials; concrete panels; ductility; durability; engineering properties; fiber-reinforced cement-based materials; ferrocement; fibers; flexural strength; glass fiber-reinforced concrete; glass fibers; manufacturing methods; mesh reinforcement; premix; toughness.

Contents: Chapter 1—Introduction and scope, p. 549.3R-2

1.1—Introduction

1.2—Scope

Chapter 2—Notation, definitions, and acronyms

p. 549.3R-2

2.1—Notation

2.2—Definitions

2.3––Acronyms

Chapter 3—Materials and mixture proportions of glass fiber-reinforced concrete premix, p. 549.3R-3

3.1—Types of premix

3.2—Typical mixture ingredients

3.3—Typical mixture proportions

Chapter 4—Properties of glass fiber-reinforced concrete premix, p. 549.3R-6

4.1—Influence of fiber content

4.2—Influence of fiber length

4.3—Influence of fiber orientation

4.4—Influence of fiber geometry

4.5—Influence of chopped fibers with reinforcing scrim

4.6—Influence of mixture proportions and mixture ingredients

4.7—Durability of glass fiber-reinforced concrete premix Chapter 5—Manufacturing processes for glass fiber-reinforced concrete premix, p. 549.3R-9

5.1—Cast premix process

5.2—Spray premix process

5.3—Press-molded premix process

5.4—Pultruded premix process

5.5—Extruded premix process

5.6—Types of equipment

5.7—Quality control considerations

Chapter 6—Applications of glass fiber-reinforced concrete premix, p. 549.3R-16

6.1—Architectural products

6.2—Industrial products

6.3—Civil engineering products

6.4—Landscaping products

6.5—Surface bonding

6.6—Stucco

6.7—Shotcrete

6.8—Glass fiber-reinforced concrete bagged products

Chapter 7—Summary, p. 549.3R-22

Chapter 8—References, p. 549.3R-22

8.1—Referenced standards and reports

8.2—Cited references


Note: You cannot mix hard copy orders with electronic downloads.

Ship a hard copy of this item to me.

Quantity:    


Download an electronic version to my computer.  


You may also be interested in these items: