Title:
Predicting Service Life of Steel-Reinforced Concrete Exposed to Chlorides
Author(s):
Dale P. Bentz, W. Spencer Guthrie, Scott Z. Jones, and Nicos S. Martys
Publication:
Concrete International
Volume:
36
Issue:
9
Appears on pages(s):
55-64
Keywords:
binding, reinforcing bar, corrosion, cracking
DOI:
Date:
9/1/2014
Abstract:
Although computer models for predicting the service life of reinforced concrete exposed to chlorides have been developed and enhanced during the past 15 years, there are many real-world considerations that complicate accurate and representative modeling of field structures. Recent advances in both concrete-specific models and general-purpose modeling platforms are permitting detailed investigations of the influences of many of these parameters. The article reviews these real-world considerations and provides some examples of how they are being addressed via advanced modeling capabilities.