Title: Concrete Q & A: Popouts or Popoffs?

Author(s):

Publication: Concrete International

Volume: 35

Issue: 12

Appears on pages(s): 88

Keywords:

Date: 12/1/2013

Abstract:
My concrete driveway was placed last year in the fall. This summer, I noticed that small concrete fragments have broken off the driveway surface exposing large pieces of aggregate. Can you tell me what might have caused this issue? Should I worry about further deterioration?