Title: Best Practices in Decorative Concrete

Author(s):

Publication: Concrete International

Volume: 35

Issue: 12

Appears on pages(s): 56-57

Keywords:

Date: 12/1/2013

Abstract:
Many traditional curing methods, such as water application by sprinkling, ponding, or absorbent materials, shouldn’t be used on decorative concrete flatwork because they will discolor the concrete.