Title: Le Toumelin

Author(s): Antoine E. Naaman and Pierre Brenet

Publication: Concrete International

Volume: 34

Issue: 11

Appears on pages(s): 31-37

Keywords:

Date: 11/1/2012

Abstract:
A ferrocement schooner with a quarter century of successful service