Title: Ensuring Performance and Durability

Author(s): Ted Neff

Publication: Concrete International

Volume: 34

Issue: 10

Appears on pages(s): 48-50

Keywords:

Date: 10/1/2012

Abstract:
New specifications released by the Post-Tensioning Institute