Title: Detailing Corner: Reinforcing Bar Layout for Two-Way Slabs

Author(s):

Publication: Concrete International

Volume: 34

Issue: 11

Appears on pages(s): 37-39

Keywords:

Date: 11/1/2012

Abstract:
In this month’s Detailing Corner, we examine the typical reinforcement layout of two-way slabs and present a number of suggestions for good detailing practices.