Title:
Discussion from the January/February 2015 ACI Structural Journal
Author(s):
José R. Martí-Vargas; and William L. Gamble
Publication:
Structural Journal
Volume:
112
Issue:
1
Appears on pages(s):
115-117
Keywords:
DOI:
10.14359/51687647
Date:
1/1/2015
Abstract:
Discussion 111-S22/From the March-April 2014 ACI Structural Journal, p. 257 Bond Strength of Spliced Fiber-Reinforced Polymer Reinforcement. Paper by Ali Cihan Pay, Erdem Canbay, and Robert J. Frosch; and Discussion 111-S25/From the March-April 2014 ACI Structural Journal, p. 291 Behavior of Epoxy-Injected Diagonally Cracked Full-Scale Reinforced Concrete Girders. Paper by Matthew T. Smith, Daniel A. Howell, Mary Ann T. Triska, and Christopher Higgins