ACI 506R-05

Guide to Shotcrete

ACI-Committee 506, technical committee document 506.R-05, 40 pp.

Order Code: 50605.NEWPUBS

Click here for more information and price

This guide provides information on materials and properties of both dry-mix and wet-mix shotcrete. Most facets of the shotcrete process are covered, including application procedures, equipment requirements, and responsibilities of the shotcrete crew. Other aspects, such as preconstruction trials, craftsman qualification tests, materials tests, and finished shotcrete acceptance tests, are also discussed.