Guide to Cold Weather Concreting
ACI Committee 306, technical committee document 306R-10, 2010, 26 pp.
Order Code: 30610.NEWPUBS
This guide discusses: concrete temperature during mixing and placing, temperature loss during delivery, preparation for cold weather concreting, protection requirements for concrete that does not require construction supports, estimating strength development, methods of protection, curing requirements, and admixtures for accelerating setting and strength gain including antifreeze admixtures.