Title:522.1-08: Specification for Pervious Concrete Pavement
Author(s):ACI Committee 522
Publication:Technical Documents
Pages:7
Keywords:concrete parking lots; concrete pavements; construction; curing; inspection testing; jointing; pavement; pervious concrete; specifications.
Date:March 1, 2008
 
Abstract:

This specification covers materials, preparation, forming, placing, finishing, jointing, curing, and quality control of pervious concrete pavement. Provisions governing testing, evaluation, and acceptance of pervious concrete pavement are included.

This reference specification can be made applicable by citing it in Project Specifications. The Architect/Engineer supplements this reference specification as needed by designating or specifying individual project requirements