Title:Confinement Model for Axially Loaded Concrete Confined by Circular Fiber-Reinforced Polymer Tubes
Author(s):Amir Z. Fam and Sami H. Rizkalla
Publication:Structural Journal
Volume:98
Issue:4
Pages:451-461
Keywords:concrete; confinement; fiber-reinforced polymer; strain; stress; tubes.
Date:July 1, 2001
 
Abstract:

An analytical model is introduced in this paper to predict the behavior of axially loaded circular concrete columns confined by fiber-reinforced polymer (FRP) tubes. The model is an extension to the confinement model introduced by Mander et al. for concrete confined by steel reinforcement. The model is based on equilibrium, compatibility conditions, and the biaxial strength failure criteria of FRP tubes. It can be used to predict the behavior of prefabricated FRP tubes totally filled or partially filled with concrete, as well as concrete wrapped with FRP sheets. The model can account for the case of axially loaded concrete core only as well as the composite section of the concrete core and FRP tube. The model is verified by experimental results reported by the authors and other researchers. A parametric study is presented to examine the effect of stiffness of the FRP tube, the effect of loading the FRP tube axially, and the effect of presence of inner hole inside the concrete core. The study showed that increasing the central hole size reduces the confinement effect, increasing the stiffness of the tube improves the confinement, and axial loading of the FRP tube significantly reduces the confinement.


Registered Subscribers: View the full article. Not an online Structural Journal subscriber? Click here to subscribe.


This document is available as a free download to qualified members.


Order Now An electronic (PDF) version is available for purchase and download. Click on the Order Now button to continue with the download.