International Concrete Research & Information Portal  
 
Title:Durability of High Alumina Cement Mortars for the Marine Environment
Author(s):N. C. Baker and P. F. G. Banfill
Publication:Special Publication
Volume:145
Pages:409-422
Keywords:admixtures; durability; high-alumina cements; marine atmospheres; mortars (material); seawater; temperature; tests; Materials Research
Date:May 1, 1994
 
Abstract:

High-alumina cement (HAC) mortars, made at 5, 20, and 40 C, were mixed using seawater, deionized water, and reconstituted seawater. The admixtures used were an accelerator, superplasticizer, antiwashout, air-entraining and waterproofing admixtures, and an ethylene-vinyl acetate (EVA) polymer latex dispersion. Results on short-term (1 year) durability against freezing and thawing and wetting and drying in all three waters are presented and compared to the performance of the same combination over 3 years at a maritime exposure site. The samples with polymer latex performed poorly in most tests, while the control and samples with accelerator and superplasticizer performed well in both laboratory exposure conditions and on the maritime site. Temperature of mixing and curing is very important in both the early and long-term performance of HAC, but the interactions between the effects of admixtures and conditions mean that it is obligatory to carry out durability tests on any proposed combination before a decision is made regarding materials selection.


Registered Subscribers: View the full article. Not an online Special Publication subscriber? Click here to subscribe.


This document is available as a free download to qualified members.


Order Now An electronic (PDF) version is available for purchase and download. Click on the Order Now button to continue with the download.