ACI - American Concrete Institute
About ACI Bookstore & Publications Certification Chapters Committees Conventions & Events Education International Membership Students Technical
  ACI Bookstore
 
Not Logged in - ATTENTION MEMBERS: You will not receive member prices until you log in
 
 
 
cart.gif (1759 bytes)
Delete Item    ITEM: RPRINTP-12247
ci2702abou-zied.pdf
ELEC
$25.00 .... $25.00

Delete Item    ITEM: RPRINTP-15514
ci0801wilson.pdf
ELEC
$25.00 .... $25.00

Delete Item    ITEM: RPRINTP-9400
ci2603amick.pdf
ELEC
$25.00 .... $25.00

Delete Item    ITEM: RPRINTP-8089
ci2110rizkalla.pdf
ELEC
$25.00 .... $25.00

Delete Item    ITEM: RPRINTP-11755
ci2612whittier.pdf
ELEC
$25.00 .... $25.00

TOTAL: $125.00
Clear Cart

Check Out

 
Instructions:

Click delete to delete item.

Member Prices
To receive member prices on the Bookstore you must be registered. If you have already registered and are not receiving member prices, you may need to log-in.

Resume Downloads
If for some reason you lose your connection while downloading a document you can resume the download by clicking on this link.

PDF Portable Document Format
All documents available for download are stored in PDF format and require a PDF reader to view them. You may download the free Adobe Acrobat Reader at the following link.  

 

 

Download an electronic version to my computer.  

This item is also available as hard copy.



 
You may also be interested in these items:
311.6M-09 Specification for Ready Mixed Concrete Testing Services (METRIC)
201.1R-08 Guide for Conducting a Visual Inspection of Concrete in Service
SP-002(07) Manual of Concrete Inspection
311.4R-05: Guide for Concrete Inspection
350.1-01/350.1R-01: Tightness Testing of Environmental Engineering Concrete Structures & Commentary
304.3R-96: Heavyweight Concrete: Measuring, Mixing, Transporting, and Placing (Reapproved 2004)

Title: 311.6-09 Specification for Ready Mixed Concrete Testing Services

Author: Committee 311
Year of Publication: 2009
Number of Pages: 5
This document is: Active
Nonmember Price: $31.50
ACI Member Price: $19.00
Order Code: 311609

Abstract: This Reference Specification covers Testing Agency requirements for field and laboratory testing of ready mixed concrete delivered to the project. It is intended for use by specifiers, architects, engineers, owners, contractors, and other groups interested in monitoring the quality of concrete used in project construction. This Reference Specification can be made applicable to any construction project by citing it in a Contract. The Specifier supplements the provisions of this Reference Specification as needed by specifying individual project requirements in the Contract.

Keywords: air content; laboratory; ready mixed concrete; sampling;slump; specification; technician; temperature; testing; unit weight.

Contents: CONTENTS

(mandatory portion follows)

Section 1—General requirements, p. 311.6-2

1.1—Scope

1.2—Qualifications

1.3—Definitions

1.4—Referenced standards

1.5—Certification and accreditation organizations

1.6—Units of measurement

Section 2—Testing of ready mixed concrete,

p. 311.6-3

2.1—Sampling

2.2—Frequency of sampling and testing

2.3—Tests

2.4—Number of strength test specimens

2.5—Curing of strength test specimens

2.6—Testing for strength

Section 3—Submittals, p. 311.6-3

3.1—Scope

3.2—Reports

3.3—Report information

(mandatory portion follows)

Notes to Specifier, p. 311.6-4

General notes

Foreword to checklists, p. 311.6-4

Mandatory Requirements Checklist, p. 311.6-5

Optional Requirements Checklist, p. 311.6-5

Submittals Checklist, p. 311.6-5



Download an electronic version to my computer.  

This item is also available as hard copy.