SP-274 Fiber Reinforced Self-Consolidating Concrete: Research and Applications CD
Year of Publication: 2010
Number of Pages: 160
This document is: Active
Nonmember Price: $65.50
ACI Member Price: $40.00
Order Code: SP274CD
ISBN: 9780870313981
Category: Fiber-Reinforced Concrete
Formats: Optical Disk

Ship a CD-ROM of this Item to me.

Quantity:    

Abstract: Editors: Corina-Maria Aldea and Liberato Ferrara

Sponsored by: ACI Committees 544 and 237

This symposium CD contains eight papers that were presented at technical sessions sponsored by ACI Committees 544 and 237 at the 2009 ACI Fall Convention in New Orleans, LA. The topics of the papers cover aspects ranging from mixture composition and influence of fibers on the fresh state performance to the connection between fresh state behavior, fiber dispersion and orientation and mechanical properties of the fiber-reinforced composite to full-scale testing and development of prototype applications for structures and infrastructures.

Note: The individual papers are also available as .pdf downloads. Please click on the following link to view the papers available, or call 248.848.3800 to order.

VIEW THE PAPERS

Contents: SP-274—1

Flow Characteristics of Macro-Synthetic Fiber-Reinforced Self-Consolidating Concrete

by D. Forgeron and A. Omer

SP-274—2

Maximum Fiber Content and Passing Ability of Self-Consolidating Fiber-Reinforced Concrete

by S. Grünewald and J.C. Walraven

SP-274—3

Prediction of Stress Development and Cracking in Steel Fiber-Reinforced Self-Compacting

Concrete Overlays Due to Restrained Shrinkage

by J. Carlswärd and M. Emborg

SP-274—4

Tensile Behavior of Steel Fiber-Reinforced Self-Compacting Concrete

by V. M. C. F. Cunha, J. A. O. Barros, J.a-Cruz

SP-274—5

Investigation of Steel and Polymer Fiber-Reinforced Self-Consolidating Concrete

by M. C. Brown, H. C. Ozyildirim, and W. L. Duke

SP-274—6

Experience with Self-Consolidating High-Performance Fiber-Reinforced Mortar and Concrete

by W.-C. Liao, S.-H. Chao, and A. E. Naaman

SP-274—7

Design and Construction Aspects of Steel Fiber-Reinforced Concrete Elevated Slabs

by B. Mobasher and X. Destrée

SP-274—8

Self-Consolidating High Performance SFRC: An Example of Structural Application in Italy

by L. Ferrara, M. di Prisco, and N. Ozyurt